Under traditional repair methods, patching requires a minimum of two-inch demolition in the affected area. Besides, patching a ceiling poses an added challenge - lack of adhesion, and non-specialized material falling out. 


The use of our unique products, Polyforce Plus Adhesive, and Polyforce Polymer Cement, permits thin-patch applications, even on walls and ceilings. The combination of Polyforce Plus Adhesive and Polymer Cement creates a monolithic patch which is able to restore structural integrity of repaired slab.


Our patching process is as follows:

  1. Delaminated and unsound concrete is removed.

  2. Polyforce Plus Adhesive is applied as an adhesive layer. Its impressive 1.85 MPa adhesive strength ensures monolithic adhesion

  3. Within 40 minutes, the actual patch is applied. On very thin patches (less than a ¼ of an inch), Polyforce Polymer Cement is used; otherwise, regular cement.